COLOR-DEK COLOR QUARTZ FLOORING


LABORATORY TEST REPORTS - Base Coat(s)
Physical Properties
Test
Results
Compressive Strength
ASTM-D-695
17,500 psi
ASTM-C-579
12,500 psi
Tensile Strength
ASTM-D-638
7400 psi
ASTM-C-307
3600 psi
Flexural Strength
ASTM-D-790
13,200 psi
ASTM-C-580
5800 psi
Hardness (Shore D)
ASTM-D-2240
85
Heat Deflection Temperature
ASTM-D-648
68 ° C / 154.4 ° F
Abrasive Resistance
ASTM-D-4060
20 mg / .02 grams

LABORATORY TEST REPORTS - Top Coat(s)
Physical Properties
Test
Results
Compressive Strength
ASTM-D-695
16,300 psi
Tensile Strength
ASTM-D-638
7800 psi
Flexural Strength
ASTM-D-790
11,600 psi
Hardness (Shore D)
ASTM-D-2240
82
Heat Deflection Temperature
ASTM-D-648
63 ° C / 145.4 ° F
Abrasive Resistance
ASTM-D-4060
24 mg / .024 grams